The manufacture of samarium cobalt alloys via the co-reduction of an oxide mix is a specialised process yielding very fine-grained high performance alloy powders. Co-reduction has now become the industry standard for SmCo5 production; the capability of this process also extends to the manufacture of Sm2Co17 powders, where the product type can provide significantly improved processing performance for customers.
printable version
click here to download the Acrobat Reader.

Compositions and Purity

(Weight %) SmCo5 Sm2Co17

Sm 33.0 - 42.0 24.0 - 30.0
Fe 14.0 - 19.0
Cu 4.0 - 8.0
Zr 1.5 - 3.5
Co Balance Balance
Calcium <0.15 <0.15
Nickel <0.20 <0.20
Iron <0.20
Aluminium <0.05 <0.05
Silicon <0.05 <0.05
Magnesium <0.03 <0.03
Boron <0.0005 <0.0005
Oxygen <0.30 <0.30
Carbon <0.030 <0.060


Individual compositions are usually set by the end-user, with alloys manufactured and supplied to specifications agreed between LCM and the customer.


Alloying additions
Praseodymium and Gadolinium are common rare-earth additions to these Sm-Co based alloy systems.

Form
A dark grey powder, particle size 100% <300µm

Quantity
Batch sizes range from 200kg to 2000kg

Packaging
Inner: Vacuum-Sealed multilayer aluminised laminate packs. This packaging provides excellent shelf life with protection from oxygen and humidity.
Outer: UN Steel drums 50-100kg net weight

Quality assurance
Production processes are part of our quality management system – certified to ISO9001: 2000 standard. Each batch is supplied with a Certificate of Conformance detailing the results from full chemical analysis and, if required, powder size distribution.